Physical Properties of 347/347H Alloys in the Annealed Condition at -20°F to +100°F
|
|
|
Tensile Strength |
Yield Strength |
|
|
|
|
|
|
Alloy |
UNS Designation |
Spec. |
psi |
MPa |
ksi |
psi |
MPa |
ksi |
Elongation in 2 inches (min.) % |
Grain Size Req. |
Maximum Harndess |
Modulus of Elasticity(x106psi) |
Mean Coefficient of Thermal Expansion (IN./IN./°F x 10-6) |
Thermal Conductivity (BTU-in/ft2-h-°F) |
347 |
S34700 |
— |
75,000 |
515 |
— |
30,000 |
205 |
— |
35 |
— |
— |
29.0 |
9.2 |
— |
347H |
S34709 |
— |
75,000 |
515 |
— |
30,000 |
205 |
— |
35 |
7 or coarser |
— |
29.0 |
9.2 |
— |
Composition of 347/347H tubing and pipe
Grade |
347 |
347H |
UNS Designation |
S34700 |
S34709 |
Carbon (C) Max. |
0.08 |
0.04–0.10 |
Manganese (Mn) Max. |
2.00 |
2.00 |
Phosphorous (P) Max. |
0.04 |
0.04 |
Sulphur (S) Max. |
0.03 |
0.03 |
Silicon (Si) Max. |
0.75 |
0.75 |
Chromium (Cr) |
17.0–20.0 |
17.0–20.0 |
Nickel (Ni) |
9.0–13.0 |
9.0–13.0 |
Molybdenum (Mo) |
— |
— |
Nitrogen (N) |
— |
— |
Iron (Fe) |
Bal. |
Bal. |
Other Elements |
Cb+Ta=10xC-1.0 |
Cb+Ta=8xC-1.0 |
347/347H Product Range
Alloy |
UNS Designation |
Werkstoff NR. |
Specifications* |
347 |
S34700 |
1.4550 |
A269, A/SA249, A/SA312 |
347H |
S34709 |
— |
A/SA249, A/SA312
|
|
|
|
|
Product Image
|